A Study of the Shrinkage Reduction in High Performance Concrete according to the Adding Ratio of Anti-Shrinkage Agent

수축저감제 혼입률 변화에 따른 고성능 콘크리트의 수축저감에 관한 연구

  • 한천구 (청주대학교 건축공학부) ;
  • 김호림 (청주대학교 대학원) ;
  • 문학용 (청주대학교 대학원) ;
  • 강수태 (한국건설기술연구원 구조연구부) ;
  • 고경택 (한국건설기술연구원 구조연구부) ;
  • 김도겸 (한국건설기술연구원 구조연구부)
  • Published : 2003.11.01

Abstract

This study discusses the use of anti-shrinkage agent as the method to reduce autogenous and drying shrinkage. According to results, as for the fundamental properties of high performance concrete, fluidity and strength decrease with an increase of the adding ratio of anti-shrinkage agent, but air content increases. Compared with plain concrete, autogenous and drying shrinkage are reduced by 12~52% and 4~22% respectively upto the adding rario of anti-shrinkage agent of 2.0%. When expansive additive is added by 5.0%, they are also reduced by 38~95% and 15~50% respectively. Therefore, as expansive additive of 5.0% and anti-shrinkage agent of 1.0% are added to high performance concrete of around W/B 30%, it is considered that fluidity and strength are hardly influenced, and in addition, crack by shrinkage can be prevented effectively.

Keywords