Strength Properties of Polymer-Modified Mortar with High-Range Water- Reducing Agents

고성능 감수제를 첨가한 폴리머 시멘트 모르타르의 강도 특성

  • 이윤수 (주성대학 콘크리트 보수ㆍ보강재료 연구소) ;
  • 주명기 (주성대학 콘크리트 보수ㆍ보강재료 연구소)
  • Published : 2003.05.01

Abstract

The effects of high-range water-reducing agent (WRA) content and polymer-cement ratio on the strength properties of autoclaved SBR-modified mortars with WRA are examined. As a result, the flexural strength of the autoclaved SBR-modified mortars with WRAs tends to increase with increasing WRA content and polymer-cement ratio, and reaches a maximum at a WRA content of 2.0%. The compressive strength of the autoclaved SBR-modified mortars with WRAs is inclined to increase with increasing WRA content and polymer-cement ratio, and reaches a maximum at a WRA content of 2.0% and a polymer-cement ratio of 10%. From the test results, the addition of the WRAs is effective for improving strength properties of the autoclaved SBR-modified mortars.