Etching behaviors of ferroelectric $YMnO_3$ thin films were studied by an inductively coupled plasma (ICP). Etch characteristic on ferroelectric $YMnO_3$ thin film have been investigated in terms of etch rate, selectivity and etch profile. The maximum etch rate of $YMnO_3$ thin film is $300{\AA}/min$ at $Ar/Cl_2$ of 2/8, RF power of 800W, dc bias voltage of 200V, chamber pressure of 15mTorr and substrate temperature of $30^{\circ}C$. Addition of $CF_4$ gas decrease the etch rate of $YMnO_3$ thin film. From the results of XPS analysis, YFx compounds were found on the surface of $YMnO_3$ thin film which is etched in $Ar/Cl/CF_{4}$ plasma. The etch profile of $YMnO_3$ film is improved by addition of $CF_4$ gas into the $Ar/Cl_2$ plasma. These results suggest that fluoride yttrium acts as a sidewall passivants which reduce the sticking coefficient of chlorine on $YMnO_3$.

Keywords