Engineering Properties of Fly Ash-WFS Mixed Materials as a Flow able Backfill
유동성 뒷채움재로 사용하기 위한 플라이에쉬-폐주물사 혼합재료의 특성 연구
Abstract
The objective of this study is to present engineering properties required in use of co-mixtures of fly ash and WFS(Waste Foundry Sand)'s, which are Presently used as fill or (lovable backfill. The fly ash, generated at the Tae-An thermoelectric power plant was used in this research and was classified as Class F. Green Sand, Furane Sand, and Coated Sand, which had been used at a foundry located in Pusan, were used. Laboratory experiments were peformed to obtain the physical properties of the co-mixture of fly ash and WFS. The range of permeability for all the co-mixtures was from 3.0×10/sup -3/㎝/s to 6.0×10/sup -5/㎝/s. The unconfined strength of the 7-day cured specimens composed of Green Sand reached 94% of that of 28-day cured specimens but for the 7-day cured specimens composed of, respectively, Furnace Sand and Coated Sand, only 64% and 66% of the strength of the 28-day cured specimens were reached. Results of the consolidated-untrained triaxial test showed that the specimens composed of Furnace Sand showed a distinct increase of the internal friction angle, while the other specimens showed negligible increase. In the case of 28-day cured specimens, specimens composed of Furnace Sand showed an internal friction angle of 41.8°, while specimens of Green and Coated Sand showed those of 33.5° and 35.0°, respectively. From the shrinkage test, the shrinkage ratios of all specimens did not exceed 0.25%.