A Fundamental Study on the Properties of Lightweight Mortar Mixed with Bottom ash and Waste Foundry Sand

괴상석탄재와 폐주물사를 혼입한 경량모르터의 특성에 관한 기초적 연구

  • Published : 1997.10.01

Abstract

In this study, bottom ash, lightweight aggregate, and Expanded Polystyrene was used to lighten the mortar. In order to compensate the reduction of strength caused by lightening, the waste foundry sand produced as solid waste was substituted for fine aggregate. As the device of reducing the ratio of absorption, the procedure of mixture was altered to check the effectiveness of surface coating of porous lightweight aggregate. It was observed over 170kg/$\textrm{cm}^2$ compressive strength at gravity about 1.3, an over 380kg/$\textrm{cm}^2$ at gravity about 1.7. the maximum strength was occurred when 30% of fine aggregate was replaced was replaced with waste foundry sand, and the ratio of absorption was decreased over 10% by changing the procedure of mixture.