Properties of Superplasticized Ready Mixed Concrete for Heavily Reinforced Concrete Structure

철근배근이 복잡한 구조물에 타설하기 쉬운 초유동 레미콘 특성

  • 조일호 (동양시멘트(주) 고객지원부 대리) ;
  • 신무섭 (동양시멘트(주) 고객지원부장) ;
  • 백일환 (동양시멘트(주) 고객지원부) ;
  • 이건갑 (동양시멘트(주) 고객지원부)
  • Published : 1997.04.01

Abstract

This research which lays emphasis on ready mixed concrete standard 25-210~240kgf/$\textrm{cm}^2$ shows the influence caused by the ratio of ingredients of superplasticized concrete, and the flowing and strength development of mortar and concrete according to the ratio of ingredients. This research shows that flowability, compactability, and segregation resistivity are the best condition under the following ratio of ingredients: fly ash 30%, unit binders 490~510kg/$\textrm{m}^3$, unit weight of water 184~194kg/$\textrm{m}^3$, fine aggregate ratio 49~51%, and superplasticizer 1.1~1.5%. Following this ratio of ingredients, the reinforced concrete structures to need design strength 25-210~240kgf/$\textrm{cm}^2$ can apply to complicated constructions.